Blown seams

Is my Yam 360s nearing the end? The plasticizing is failing in a few places. I put 3 psi in the tubes and in this hot weather the seam has blown in 3 places in the bow.
I have also discovered one of the baffles is blown.
Seemingly a seam repair involves forcing glue into the seam.
Is it worth buying the more expensive two part glue?
__________________
billows is offline   Reply With Quote
Old 15 July 2019, 23:34   #2
Member
 
Locozodiac's Avatar
 
Country: Other
Town: Lima-Peru
Boat name: Nautile
Make: Sea Rider 450 Rib
Length: 4m +
Engine: Tohatsu 5/18/30 HP
Join Date: Sep 2007
Posts: 1,998
Yes definitively, much better and stronger than one part quick repair glue. In summer you should inflate Sib much less say 2.5 PSI and don't leave Sib out of water resting on hot surfaces as sand beaches, concrete floors.

Happy Boating
__________________
Locozodiac is offline   Reply With Quote
Old 24 July 2019, 09:33   #3
Member
 
Country: Ireland
Town: ...
Boat name: none
Make: Honwave 3.5-AE
Length: 3m +
Engine: Mariner 6hp
Join Date: Jul 2011
Posts: 119
I reglued the seam leaks and it seems to be holding air. Maybe life in the old Yam yet
__________________
billows is offline   Reply With Quote
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off




All times are GMT. The time now is 18:45.


Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.