I did try applying PVA with a sponge on the first attempt. It came out Ok but I did get some imperfections. This was probably just me. I found it a lot easier to spray but I have heard of loads of people who use a sponge including the people I get my fiberglass materials off.

And yes banging can cause cracks. I have always done it that way because that is the way I was taught when I did my course. I have been lucky so far.

I think everyone develops there own way of doing things and will have their own good and bad stories to tell. I used wedges on my first attempt but no matter how hard I tried I couldn't get them in without leaving some marks.

On the course I did, I was told to leave the mould at least 3 days at room temperature. I have always left anything I have done around about a week. This works for me. I would really recommend Farecla G3 Liquid. It really does put a shine on the finished product.
__________________
slangley is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off




All times are GMT. The time now is 03:17.


Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.